Appearance (visual inspection): light yellow powder
Content,%, ≥ 98.0
Heating reduction,%, ≤ 0.40
Sieve residue (150 μ m) ,%, ≤ 0.10
Product Description: EG-3 is easy to blend and disperse in the rubber compound, and it will not cause surface frost (whitening) during vulcanization. When heated at high temperature, it can shorten the vulcanization time and effectively vulcanize EPDM, reduce the compression permanent deformation of the product, and have good high-temperature aging resistance. If a combination of peroxide and sulfur is used, it can also be used.
Application scope: A comprehensive accelerator specialized for EPDM, which can also be used for rubber products such as NBR and SBR.
Addition amount: Suggested addition amount: 3-5 parts (calculated based on the proportion of raw rubber), depending on the actual situation.
Packaging and storage: kraft paper bags, lined with plastic bags, net weight 25KG. Store in a cool and dry place with the original packaging sealed for 1 year.